Production of fine titanium powder from titanium sponge by the shuttle of the disproportionation reaction in molten NaClKCl

Materials Transactions
  • Xin Lu
  • ,
  • Takuya Ono
  • ,
  • Osamu Takeda
  • ,
  • Hongmin Zhu

60
3
開始ページ
405
終了ページ
410
記述言語
英語
掲載種別
研究論文(学術雑誌)
DOI
10.2320/matertrans.MA201811

©2019 The Japan Institute of Metals and Materials. Titanium and its alloys are key materials for various fields. Low cost and high-quality titanium powder production methods are crucial for powder metallurgy (PM) and additive manufacturing (AM) of titanium to significantly decrease the manufacturing cost. In this study, the production of titanium powder from raw material titanium sponge was achieved through the shuttle of the disproportionation reaction and the backward reaction of Ti 2+ to Ti 3+ and Ti metal in molten NaClKCl at 750°C. With the addition of a very small amount of TiCl 2 , over 7 3 70 times of titanium powder in mass comparing to the added Ti 2+ was obtained. The primary particle size of the powder formed based on the disproportionation reaction was approximately 1 µm, while the secondary agglomerated particle size was in the range of 25 3 50 µm. No significant difference of the particle size distribution was found for the experimental runs with different TiCl 2 concentrations and holding times. The proposed production method of titanium powder from titanium sponge is expected to significantly decrease the production cost of titanium powder.

リンク情報
DOI
https://doi.org/10.2320/matertrans.MA201811
URL
https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=85062391892&origin=inward
ID情報
  • DOI : 10.2320/matertrans.MA201811
  • ISSN : 1345-9678
  • SCOPUS ID : 85062391892

エクスポート
BibTeX RIS