2012年1月
Environmental leaching characteristics of scorodite synthesized with Fe(II) ions
Hydrometallurgy
- ,
- ,
- ,
- 巻
- 111-112
- 号
- 1
- 開始ページ
- 87
- 終了ページ
- 102
- 記述言語
- 掲載種別
- 研究論文(学術雑誌)
- DOI
- 10.1016/j.hydromet.2011.10.006
The leaching characteristics of scorodite particles synthesized from Fe(II) under different conditions, such as reaction time and temperature, were investigated. The solution conditions, such as pH and temperature, were changed in leaching experiments. The results showed that the leaching characteristics depend on the synthesis temperature of scorodite particles, particle size, type of solvent and so on. Since the amount of As dissolved from particles with the high Fe/As molar ratio is relatively low, the Fe/As molar ratio of the particles is an important factor to control the dissolution of As from scorodite particles. The results of leaching tests with repeated renewal solution showed that pH of solution is the most important factor in the As dissolution. It was found that the addition of goethite to the scorodite is also effective to reduce the amount of As in solution. © 2011 Elsevier B.V. All rights reserved.
- リンク情報
- ID情報
-
- DOI : 10.1016/j.hydromet.2011.10.006
- ISSN : 0304-386X
- SCOPUS ID : 84857192705